Til hvers er INCONEL notað?
Inconel efnasamsetning
| EINKIN | ÞÁTTUR (% UM MASSA) | ||||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| NI | CR | FE | MO | NB | CO | MN | CU | AL | TI | SI | C | S | P | B | |
| 600 | 72.0 | 14.0–17.0 | 6.0–10.0 | 1.0 | 0.5 | 0.5 | 0.15 | 0.015 | |||||||
| 617 | 44.2–56.0 | 20.0–24.0 | 3.0 | 8.0–10.0 | 10.0–15.0 | 0.5 | 0.5 | 0.8–1.5 | 0.6 | 0.5 | 0.15 | 0.015 | 0.015 | 0.006 | |
| 625 | 58.0 | 20.0–23.0 | 5.0 | 8.0–10.0 | 3.15–4.15 | 1.0 | 0.5 | 0.4 | 0.4 | 0.5 | 0.1 | 0.015 | 0.015 | ||
| 690 | 59.5 | 30 | 9.2 | 0.35 | 0.01 | 0.02 | 0.35 | 0.019 | 0.003 | ||||||
| 718 | 50.0–55.0 | 17.0–21.0 | jafnvægi | 2.8–3.3 | 4.75–5.5 | 1.0 | 0.35 | 0.2–0.8 | 0.65–1.15 | 0.3 | 0.35 | 0.08 | 0.015 | 0.015 | 0.006 |
| X-750 | 70.0 | 14.0–17.0 | 5.0–9.0 | 0.7–1.2 | 1.0 | 1.0 | 0.5 | 0.4–1.0 | 2.25–2.75 | 0.5 | 0.08 | 0.01 | |||
Inconel jafngild efni
| STANDAÐUR | WERKSTOFF NR. | SÞ | GOST | AFNOR | JIS | BS | EN | EÐA |
|---|---|---|---|---|---|---|---|---|
| Inconel 600 | 2.4816 | N06600 | МНЖМц 28-2,5-1,5 | NC15FE11M | NCF 600 | NA 13 | NiCr15Fe | ЭИ868 |
| Inconel 601 | 2.4851 | N06601 | XH60BT | NC23FeA | NCF 601 | NA 49 | NiCr23Fe | ЭИ868 |
| Inconel 617 | 2.4663 | N06617 | ||||||
| Inconel 625 | 2.4856 | N06625 | ХН75МБТЮ | NC22DNB4M | NCF 625 | NA 21 | NiCr22Mo9Nb | ЭИ602 |
| Inconel 690 | 2.4642 | N06690 | ||||||
| Inconel 718 | 2.4668 | N07718 | ||||||
| Inconel 725 | - | N07725 | ||||||
| Inconel X-750 | 2.4669 | N07750 |
Inconel og Monel
Inconel og Monel eru bæði nikkel-sem innihalda málmblöndur. Samt sem áður, auk þess að innihalda nikkel sem aðalblendiefni, innihalda þeir einnig aðra þætti sem aukablendiefni. Monel, til dæmis, er samsett úr kopar, sem er 30 til 40 prósent af heildarþyngd hans. Inconel inniheldur króm sem hjálparblöndunarefni. Hvað varðar eiginleika þess er Monel meðal-afköst málmblöndu en Inconel er mikil-afköst tegund. Nokkrar Inconel málmblöndur eru einnig þekktar sem ofurblöndur vegna þess að þær hafa framúrskarandi tæringarþol og standa sig betur en nokkrar hefðbundnar málmblöndur við háan hita. Monel er tvíundir málmur í föstu lausnum en Inconel er austenítískt háhitamálmblöndur.



Inconel vélrænni eiginleikar
| ÞÉTTLEIKI | Bræðslumark | STREKKSTYRKUR | ÁTVRUNARSTYRKUR (0,2%FRÆÐI) | LENGING | |
|---|---|---|---|---|---|
| 600 | 8,47 g/cm3 | 1413 gráður (2580 gráður F) | Psi – 95.000, MPa – 655 | Psi – 45.000, MPa – 310 | 40 % |
| 601 | 8,1 g/cm3 | 1411 gráður (2571 gráður F) | Psi – 80.000, MPa – 550 | Psi – 30.000, MPa – 205 | 30 % |
| 617 | 8,3g/cm³ | 1363 gráður | Stærri en eða jafnt og 485 MPa | Stærri en eða jafnt og 275 MPa | 25 % |
| 625 | 8,4 g/cm3 | 1350 gráður (2460 gráður F) | Psi – 135.000, MPa – 930 | Psi – 75.000, MPa – 517 | 42.5 % |
| 690 | 8,3g/cm³ | 1363 gráður | Stærri en eða jafnt og 485 MPa | Stærri en eða jafnt og 275 MPa | 25 % |
| 718 | 8,2 g/cm3 | 1350 gráður (2460 gráður F) | Psi – 135.000, MPa – 930 | Psi – 70.000, MPa – 482 | 45 % |
| 725 | 8,31 g/cm3 | 1271 gráðu -1343 gráður | 1137 MPa | 827 MPa | 20 % |
| X-750 | 8,28 g/cm3 | 1430 gráður | 1267 MPa | 868 MPa | 25 % |
Monel efni jafngildi
| STANDAÐUR | WERKSTOFF NR. | SÞ | GOST | AFNOR | JIS | BS | EN |
|---|---|---|---|---|---|---|---|
| Monel 400 | 2.4360 | N04400 | МНЖМц 28-2,5-1,5 | NU-30M | NW 4400 | NA 13 | NiCu30Fe |
| Monel 404 | 2.4867 | N04404 | |||||
| Monel 405 | N04404 | ||||||
| Monel K500 | 2.4375 | N05500 |
Monel efnasamsetning
| VIÐSKIPTANAFN | ASTM/AISI BÆRÐARGERÐ |
SÞ | %CU | %AL | %TI | %FE | %MN | %SI | %NI |
|---|---|---|---|---|---|---|---|---|---|
| Monel 400 | B 127, B 164 | N04400 | 28-34 | 2,5 hámark | 2,0 hámark | 0,5 hámark | 63 mín | ||
| Monel 401 | N04401 | 28-34 | 2,5 hámark | 2,0 hámark | 63 mín | ||||
| Monel 404 | N04404 | Rem | 0,05 hámark | 0,5 hámark | 0,1 hámark | 0,1 hámark | 52-57 | ||
| Monel K-500 | B 865 | N05500 | 27-33 | 2.3-3.15 | 0.35-0.85 | 2,0 hámark | 1,5 hámark | 0,5 hámark | 63 mín |
| Monel 405 | B 164 | N04405 | 28-34 | 2,5 hámark | 2,0 hámark | 0,5 hámark | 63 mín |
Monel vélrænni eiginleikar
| ÞÉTTLEIKI | Bræðslumark | STREKKSTYRKUR | ÁTVRUNARSTYRKUR (0,2%FRÆÐI) | LENGING | |
|---|---|---|---|---|---|
| Monel 400 | 8,8 g/cm3 | 1350 gráður (2460 gráður F) | Psi – 80000, MPa – 550 | Psi – 35000 , MPa – 240 | 40 % |
| Monel 404 | 8,91 g/cm3 | 1300 - 1350 gráðu | 70 KSI mín (483 MPA mín) | 25 KSI mín (172 MPA mín) | 35 % |
| Monel 405 | 8,80 g/cm3 | 1300 - 1350 gráðu | 550 MPa | 240 MPa | 40 % |
| Monel K500 | 8,44 g/cm3 | 1350 gráður (2460 gráður F) | Psi – 160000, MPa – 1100 | Psi – 115000 , MPa – 790 | 20 % |