Feb 04, 2026 Skildu eftir skilaboð

Mál og vikmörk fyrir 601 álfelgur hringlaga stangir

Mál Standard Of Inconel 601 Hringstöng

Þvermál eða
Breidd
(mm)
Þyngd á metra Hlutasvæði Jaðar
  Ferningur
(kg)
Umferð
(kg)
Ferningur
(cm²)
Umferð
(cm²)
Ferningur
(cm)
Umferð
(cm)
5.0 0.20 0.15 0.25 0.20 2.0 1.57
5.5 0.24 0.19 0.30 0.24 2.2 1.78
6.0 0.28 0.22 0.36 0.28 2.4 1.88
7.0 0.38 0.30 0.49 0.38 2.8 2.20
8.0 0.50 0.39 0.64 0.50 3.2 2.51
9.0 0.64 0.50 0.81 0.64 3.6 2.83
10 0.73 0.63 1.00 0.79 4.0 3.14
11 0.95 0.75 1.21 0.95 4.4 3.46
12 1.13 0.89 1.44 1.13 4.8 3.77
14 1.54 1.21 1.96 1.54 5.6 4.40
16 2.01 1.58 2.56 2.01 6.4 5.03
18 2.54 2.00 3.24 2.54 7.2 5.65
20 3.14 2.47 4.00 3.14 8.0 6.28
22 3.80 2.98 4.84 3.80 8.8 6.91
25 4.91 3.85 6.25 4.91 10.0 7.85
28 6.15 4.83 7.84 6.16 11.2 8.80
32 8.04 6.31 10.24 8.04 12.8 10.05
36 10.17 7.99 12.96 10.18 14.4 11.31
40 12.56 9.86 16.00 12.57 16.0 12.57
45 15.90 12.49 20.25 15.90 18.0 14.14
50 19.62 15.41 25.00 19.64 20.0 15.71
56 24.62 19.34 31.36 24.63 22.4 17.59
63 31.16 24.47 36.69 31.17 25.2 19.79
71 39.57 31.08 50.41 39.59 28.4 22.31
80 50.24 39.46 64.00 50.27 32.0 25.13

 

Inconel UNS N06601 Bright Round Bar Tolerance

Inconel 601 Round Bar Tolerance ISO "H" Series í MM
Stærð (mm) H12 H11 H10 H9 H8 H7 H6 H5
Yfir 180 - 250 +0.46/0 +0.29/0 +0.185/0 +0.115/0 +0.072/0 +0.046/0 +0.029/0 +0.02/0
Yfir 120 - 180 +0.4/0 +0.25/0 +0.16/0 +0.1/0 +0.063/0 +0.04/0 +0.025/0 +0.018/0
Yfir 80 - 120 +0.35/0 +0.22/0 +0.14/0 +0.087/0 +0.054/0 +0.035/0 +0.022/0 +0.015/0
Yfir 50 - 80 +0.3/0 +0.19/0 +0.12/0 +0.074/0 +0.046/0 +0.03/0 +0.019/0 +0.013/0
Yfir 30 - 50 +0.25/0 +0.16/0 +0.1/0 +0.062/0 +0.039/0 +0.025/0 +0.016/0 +0.011/0
Yfir 18 - 30 +0.21/0 +0.13/0 +0.084/0 +0.052/0 +0.033/0 +0.021/0 +0.013/0 +0.009/0
Yfir 10 - 18 +0.18/0 +0.11/0 +0.07/0 +0.043/0 +0.027/0 +0.018/0 +0.011/0 +0.008/0
Yfir 6 - 10 +0.15/0 +0.09/0 +0.058/0 +0.036/0 +0.022/0 +0.015/0 +0.009/0 +0.006/0
Yfir 3 - 6 +0.12/0 +0.075/0 +0.048/0 +0.03/0 +0.018/0 +0.012/0 +0.008/0 +0.005/0
~ til 3 +0.1/0 +0.06/0 +0.04/0 +0.025/0 +0.014/0 +0.01/0 +0.006/0 +0.004/0

 

Hringdu í okkur

whatsapp

Sími

Tölvupóstur

inquiry